PET monofilament yarn for forming fabric in paper making industry

PET monofilament yarn for forming fabric in paper making industry

Model No.︰VS-PM100

Brand Name︰VEKSTAR

Country of Origin︰China

Unit Price︰US $ 3 / kg

Minimum Order︰1000 kg

Inquire Now

Product Description

Product Name: PET monofilament yarn for  forming fabric in paper making industry

Material: 100% polyester

Specification: 0.20mm to 1.2mm

Luster: semidull

Color: raw white, varied dope dyed colors as per request.

Advantage and Characteristics: We specially equipped Germany standard extruding lines to produce the excellent quality polyester monofilament yarns for paper making industry. High tenacity, excellent diameter evenness, excellent friction endurance, low shrinkage.

End use and technical properties are as following:
 

1. Polyester monofilament for paper making forming fabric and dryer fabric --Weft Yarn

 

 

Model

Diameter

(mm)

Diameter deviation

(mm)

Breaking strength

(N) ≥

Tenacity

(CN/Tex), ≥

Elongation at break

(%)

Free shrinkage in hot air@ 180℃ x10min (%)

VS50F

0.22

±0.005

21

40

40±6

2±0.5

0.24

±0.005

25

40

40±6

2±0.5

0.25

±0.005

27

40

40±6

2±0.5

0.27

±0.005

32

40

40±6

2±0.5

0.30

±0.005

39

40

40±6

2±0.5

0.35

±0.006

53

40

40±6

2±0.5

0.38

±0.006

59

38

40±6

2±0.5

VS50R

0.40

±0.01

66.0

38

40±6

3±0.7

0.45

±0.012

83.0

38

40±6

3.5±0.7

0.50

±0.015

92.0

34

40±6

3.5±0.7

0.55

±0.015

111.0

34

40±6

3.5±0.7

0.60

±0.015

129.0

33

40±6

3.5±0.7

0.65

±0.015

151.0

33

40±6

3.5±0.7

0.68

±0.015

165.0

33

40±6

3.5±0.7

0.70

±0.018

170.0

32

40±6

3.5±0.7

0.80

±0.02

222.0

32

40±6

3.5±0.7

0.90

±0.025

281

32

40±6

3.5±0.7

1.0

±0.03

336

31

40±6

4±1

1.1

±0.03

407

31

40±6

4±1

1.2

±0.03

484

31

40±6

4±1

 

Features :

Medium and high molecular, anti-hydrolysis, anti-dirty, low shrinkage and medium low shrinakge.

End use: as weft yarn for paper making fabric and dryer fabric.

 

2. Polyester monofilament for paper making forming fabric and dryer fabric--Warp Yarn

 

Model

Diameter

(mm)

Diameter deviation

(mm)

Breaking strength

(N) ≥

Tenacity

(CN/Tex), ≥

Elongation at break

(%)

Free shrinkage in hot air@ 180℃ x10min (%)

VS60F

0.20

±0.005

23.0

53

16±3

12±1

0.21

±0.005

25.0

53

16±3

12±1

0.22

±0.005

28.0

53

16±3

12±1

0.23

±0.005

31.0

53

16±3

12±1

0.25

±0.005

36.0

53

16±3

12±1

0.27

±0.005

42.0

53

16±3

12±1

0.30

±0.005

52.0

53

16±3

12±1

VS60R

0.32

±0.006

59.0

53

16±3

12±1

0.35

±0.006

70.0

53

16±3

12±1

0.40

±0.001

92.0

53

16±3

12±1

0.65

±0.015

210.0

46

20±3

11±1

0.68

±0.015

230.0

46

20±3

11±1

 

Features :

Medium and high molecular, anti-hydrolysis, anti-dirty, high tenacity, medium shrinakge.

End use: as weft yarn for paper making fabric and dryer fabric.

 

3. Polyester monofilament for spiral net --Pin Yarn

 

Model

Diameter

(mm)

Diameter deviation

(mm)

Breaking strength

(N) ≥

Tenacity

(CN/Tex), ≥

Elongation at break

(%)

Free shrinkage in hot air@ 180℃ x10min (%)

VS70A

0.70

±0.018

175.0

33

30±5

8±1

0.80

±0.018

229.0

33

30±5

8±1

0.90

±0.02

272.0

31

30±5

8±1

1.0

±0.03

336.0

31

30±5

8±1

Features :

Medium molecular, medium shrinkage.

End use: as pin yarn for paper making spiral net.

 

4. Polyester monofilament for spiral net --Loop Yarn

 

Model

Diameter

(mm)

Diameter deviation

(mm)

Breaking strength

(N) ≥

Tenacity

(CN/Tex), ≥

Elongation at break

(%)

Free shrinkage in hot air@ 180℃ x10min (%)

VS70B

0.50

±0.015

114.0

42

19±3

17±1

0.60

±0.015

164.0

42

19±3

17±1

0.68

±0.015

185.0

37

19±3

17±1

0.70

±0.018

191.0

36

19±3

17±1

Features :

Medium molecular, high shrinkage.

End use: as loop yarn for paper making spiral net.